Material

Body Aluminum(5050 5052 5056 5154) (AL Mg 1%-1.5%, 2%-2.5% ,3%-3.5%,5%)
Finish Polished RAL Colour Painted
Mandrel Aluminum ● Steel Stainless Steel
Finish Polished ● Zinc Plated Polished
Head Type Dome, CSK, Large Flange

Specification

Aluminum rivet
D1
NOM.
DRILL NO.
&HOLE SIZE
ART.CODE GRIP RANGE L(MAX) D
NOM.
K
MAX.
P
MIN.
SHEAR
LBS
TENSILE
LBS
INCH MM INCH MM
3/32"
2.4mm
#41
2.5-2.6
AA32 0.020-0.125 0.5-3.2 0.250 6.4 0.188"
4.8
0.032"
0.81
1.00"
25.4
70
310N
80
360 N
AA34 0.126-0.250 3.2-6.4 0.375 9.5
AA36 0.251-0.375 6.4-9.5 0.500 12.7
1/8"
3.2mm
#30
3.3-3.4
AA41 0.020-0.062 0.5-1.6 0.212 5.4 0.250"
6.4
0.040"
1.02
1.06"
27
120
530 N
150
670 N
AA42 0.063-0.125 1.6-3.2 0.275 7.0
AA43 0.126-0.187 3.2-4.8 0.337 8.6
AA44 0.188-0.250 4.8-6.4 0.400 10.2
AA45 0.251-0.312 6.4-7.9 0.462 11.7
AA46 0.313-0.375 7.9-9.5 0.525 13.3
AA48 0.376-0.500 9.5-12.7 0.650 16.5
AA410 0.501-0.625 12.7-15.9 0.775 19.7
5/32"
4.0mm
#20
4.1-4.2
AA52 0.020-0.125 0.5-3.2 0.300 7.6 0.312"
7.9
0.050"
1.27
1.06"
27
190
850 N
230
1020 N
AA53 0.126-0.187 3.2-4.8 0.362 9.2
AA54 0.188-0.250 4.8-6.4 0.425 10.8
AA56 0.251-0.375 6.4-9.5 0.550 14.0
AA58 0.376-0.500 9.5-12.7 0.675 17.1
AA510 0.501-0.625 12.7-15.9 0.800 20.3
AA516 0.876-1.000 22.2-25.4 1.175 29.8
3/16"
4.8mm
#11
4.9-5.0
AA62 0.020-0.125 0.5-3.2 0.325 8.3 0.375"
9.5
0.060"
1.52
1.06"
27
260
1160 N
320
1430 N
AA63 0.126-0.187 3.2-4.8 0.387 9.8
AA64 0.188-0.250 4.8-6.4 0.450 11.4
AA66 0.251-0.375 6.4-9.5 0.575 14.6
AA68 0.376-0.500 9.5-12.7 0.700 17.8
AA610 0.501-0.625 12.7-15.9 0.825 21.0
AA612 0.626-.0750 15.9-19.1 0.950 24.1
AA614 0.751-0.875 19.1-22.2 1.075 27.3
AA616 0.875-1.000 22.2-25.4 1.200 30.5
AA618 1.001-1.125 25.4-28.6 1.325 33.7
AA620 1.126-1.250 28.6-31.8 1.450 36.8
1/4"
6.4mm
F
6.5-6.6
AA82 0.020-0.125 0.5-3.2 0.375 9.5 0.500"
12.7
0.080"
2.03
1.25"
32
460
2050 N
560
2500N
AA84 0.126-0.250 3.2-6.4 0.500 12.7
AA86 0.251-0.375 6.4-9.5 0.625 15.9
AA88 0.376-0.500 9.5-12.7 0.750 19.1
AA810 0.501-0.625 12.7-15.9 0.875 22.2
AA812 0.626-0.750 15.9-19.1 1.000 25.4
AA814 0.751-0.875 19.1-22.2 1.125 28.6
AA816 0.876-1.000 22.2-25.4 1.250 31.8
AA818 1.001-1.125 25.4-28.6 1.375 34.9

Application

Our full aluminum open end rivet uses high quality aluminum alloy wires. After the riveting, It will never rust. compared with ordinary rivets, the rivet intensity is low, so it is suitable for connected the soft material.Aluminum pop rivets can be divided into a dome head rivet,countersunk rivets and large flange head rivet.And the aluminum alloy material have multi choice of alu mg 2% 2.5% 3.5% and 5%(5052 5154 5056).

Fixpal open type pop rivets have the advantages of easy operation, excellent riveting, beautiful appearance, high physical properties. Perfect choice of single -sided riveting.Aluminum pop rivets can be widely used in various vehicles, vessels, machinery manufacturing, electronics, instrumentation, food machinery, medical equipment, construction, decoration and other fastening areas.

aluminum rivets

The problems and reasons when using the blind rivet:
1. Burrs: After riveting, the breaked mandrel with burrs pass through the rivet holes; or the riveting holes protrudes from the outside to form a spatula burr.
The cause of the burrs: the diameter of the mandrel is small; the rivet material is soft; the drilling hole diameter of the workpiece is too large; the muzzle specifications of the rivet gun are too large;

2. The nail head falls off: After the rivet is pulled, the core rivet head cannot be wrapped and falls off from the rivet.
The reasons for falling the rivet head of the core are: the diameter of the nail cap is too large; the rivet is shorter, and the rivet thickness does not match.

3. the rivet cracking: After the riveting, the rivet is pulsed or completely ruptured.
The reasons for the cracking of the rivet are: excessive hardness after riveting annealing or unheated treatment, the nail core hat is too large.